· Wet highintensity magnetic separation of this % Mn ore achieved a salable grade of % Mn at a recovery of %. Roasting reduction of this ore with coal produced a new Mn–Fe oxide phase that exhibited a mix of ferromagnetic and paramagnetic behavior, thereby increasing the magnetic susceptibilities by almost two orders of magnitude. The maximum grade of roasted ore that .